Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 304 - 327 °C | 580 - 620 °F | |
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristics: High Str.. |
|||
Melt Temperature | 270 - 327 °C | 518 - 620 °F | Average value: 303 °C Grade Count:45 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Melt Temperature | 299 - 327 °C | 570 - 621 °F | Excellent Processability |
Chevron Phillips 1025 Extrusion Coating Resin
(discontinued **) Resin Type: Speed Resin, Base Resin Type - Chevron PE1017Characteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF.. |
|||
Melt Temperature | 299 - 327 °C | 570 - 621 °F | Excellent Processability |
Chevron Phillips 1028 Extrusion Coating Resin
(discontinued **) Resin Type: High Speed Slip ResinCharacteristics: Excellent Processability at 570-620°F (300-325°C) Melt, Good Adhesion at Low Coating Weights and High Speed Lines, Low COF uses, FDA Approved for .. |
|||
Melt Temperature | 274 - 327 °C | 525 - 621 °F | Average value: 301 °C Grade Count:8 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Temperature | 316 - 327 °C | 600 - 620 °F | Molding |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 310 - 327 °C | 590 - 620 °F | |
LyondellBasell Petrothene® NA205000 Low Density Polyethylene, Extrusion Coating Grade Petrothene NA205000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a low coating weight at line speeds in excess of.. |
|||
Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
Styron EMERGEâ„¢ 4530-6 Polycarbonate EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Melt Temperature | 299 - 327 °C | 570 - 621 °F | |
Styron EMERGEâ„¢ 4800-7 Polycarbonate EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar.. |
|||
Melt Temperature | 299 - 327 °C | 570 - 620 °F | |
Chevron Phillips MarFlex® 1023 LDPE Extrusion Coating Resin Resin Type: Base, SpeedCharacteristics: Good adhesion at low coating weights and high line speedsLow COF usesFDA approved for food contactApplications: Can be used in the outer coextrusion layer or .. |
|||
Melt Temperature | 315 - 327 °C | 599 - 621 °F | Extrusion Coating Processability |
Dow 4012 Low Density Polyethylene (LDPE) Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow |
|||
Melt Temperature | 304 - 327 °C | 580 - 620 °F | Molding |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |