Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 166 - 210 °C | 330 - 410 °F | Average value: 188 °C Grade Count:4 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Melt Temperature | 166 - 188 °C | 330 - 370 °F | Average value: 177 °C Grade Count:3 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8915-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8925-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8940-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8950-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8999-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9077-80 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9077-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9600-80 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9915-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9925-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9950-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9980-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9999-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3200-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3201-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3300-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 90-A472R-55-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8553 Moldings & Extrusions Flexible PVC A general purpose profile extrusion compound with excellent weathering properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8644 Moldings & Extrusions Flexible PVC General purpose extrusion compound. Forms a good bond with rigid PVC in co-extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 14750 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 1601 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 7810 Moldings & Extrusions Flexible PVC 105°C rated injection molding compound approved for 94 V-0 in black and white at 0.75 mm and also approved for 94 V-0 in all colors at 1.5 mm.Information provided by Georgia GulfGeorgia Gulf became.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8603 Moldings & Extrusions Flexible PVC A soft extrusion compound with rubber-like properties and oil resistance. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8757 Moldings & Extrusions Flexible PVC Soft, general purpose, highly filled extrusion compound recommended for cove base moldings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 83-126K Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-D LLDPE