Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Temperature | 304 - 343 °C | 579 - 649 °F | |
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c.. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® A-4122 NL WH 905 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhi.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | Injection |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Melt Temperature | 290 - 343 °C | 554 - 650 °F | Average value: 319 °C Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat.. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional .. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Dry) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PC731 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Melt Temperature | 280 - 343 °C | 536 - 650 °F | Average value: 316 °C Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |
|||
Melt Temperature | 329 - 343 °C | 624 - 649 °F | |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)
(Unverified Data**) Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad.. |