Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 349 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 332 - 349 °C
630 - 660 °F
Oxford Polymers Polysulfone PSF P170-64170 White PSU
Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio..
Melt Temperature 321 - 349 °C
610 - 660 °F
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Melt Temperature 332 - 349 °C
630 - 660 °F
Molding
PolyOne Edgetek® MLS-10GF/000 Polysulfone Alloy - 10% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Melt Temperature 332 - 349 °C
630 - 660 °F
Stock
PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material  (discontinued **)
Data provided by PolyOne.
Melt Temperature 332 - 349 °C
630 - 660 °F
MTI ThermoStran® PPA-40C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Melt Temperature 332 - 349 °C
630 - 660 °F
MTI ThermoStran® PPA-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Melt Temperature 343 - 349 °C
649 - 660 °F
Solvay Specialty Polymers PrimoSpire® PR-250 Polyphenylene, Self-Reinforced (SRP)
PrimoSpire® PR-250 resin is an injection molding grade of self-reinforced polyphenylene (SRP). PrimoSpire® SRP is an ultra-high performance amorphous, melt-processable polymer. The unique prop..
Melt Temperature 332 - 349 °C
630 - 660 °F
Molding
PolyOne Edgetek® MLS-20GF/000 Polysulfone Alloy - 20% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Melt Temperature 332 - 349 °C
630 - 660 °F
Molding
PolyOne Edgetek® MLS-XC195C-2 Polysulfone Alloy - ESD Material - Lubricated  (discontinued **)
Data provided by PolyOne.
Melt Temperature 321 - 349 °C
610 - 660 °F
Molding
PolyOne Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp  (discontinued **)
Information provided by PolyOne™ Corporation
Copyright © lookpolymers.com All Rights Reserved