Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 185 - 205 °C | 365 - 401 °F | |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Melt Temperature | 185 °C | 365 °F | |
NatureWorks® Ingeo™ AW 240D Biopolymer for Food Serviceware NatureWorks® PLA polymer AW 240D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed .. |
|||
Melt Temperature | 185 - 210 °C | 365 - 410 °F | |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Melt Temperature | 185 - 220 °C | 365 - 428 °F | Recommended |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
Melt Temperature | 185 - 200 °C | 365 - 392 °F | |
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat.. |
|||
Melt Temperature | 185 - 191 °C | 365 - 376 °F | |
PolyOne Geon™ Vinyl Flexible R4294U Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 185 - 210 °C | 365 - 410 °F | |
Premix Thermoplastics PRE-ELEC® 12-031
(discontinued **) PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Melt Temperature | 185 - 366 °C | 365 - 690 °F | Average value: 258 °C Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Melt Temperature | 185 - 225 °C | 365 - 437 °F | Injection Molding |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 185 - 225 °C | 365 - 437 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1033D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 185 - 220 °C | 365 - 428 °F | |
KEP Kepital® F20 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 185 - 220 °C | 365 - 428 °F | |
KEP Kepital® F30 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 185 °C | 365 °F | |
Teknor Apex APEX® 3202-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Melt Temperature | 185 °C | 365 °F | Extrusion |
Lubrizol Estane® ALR CL57D Thermoplastic Polyurethane Type: Estane® ALR CL570 is an aliphatic, polycaprolactone-based TPU with a Shore D Durometer of 57.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin.. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 10790 Wire & Cable Flexible PVC 60C compound suitable for integral non-metallic conduit jacket 1" and larger per UL 1660.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 12880 Coax & Telecom Flexible PVC VW-1 coax cable jacket. RG 6.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 37740 Wire & Cable Flexible PVC 90°C rated compound designed for use as an inner and outer jacket in Teck 90 cables.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 38900 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 38951 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 8800 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 8810 Moldings & Extrusions Flexible PVC Low gravity extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required. Exhibits good flex whitening resistance.Information pro.. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 8830 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, shapes, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 8835 Moldings & Extrusions Flexible PVC General purpose extrusion compound with low gloss surface finish.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 - 196 °C | 365 - 385 °F | |
PolyOne Geon™ Vinyl Flexible R242AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 1055 Wire & Cable Flexible PVC NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 22883 Coax & Telecom Flexible PVC Flexible, matte-finish, flame retardant jacket compound suitable for "patch cable" constructions over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Melt Temperature | 185 °C | 365 °F | |
Axiall 4425 Flexible PVC Non-lead stabilized high speed TWP automotive insulation. Rated for a maximum service temperature of 85°C. Suitable for SAE J1128, SAE 1560, Ford MIL 120A and Chrysler MS 7889; MS-DC16 Type A.Inf.. |