Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 155 - 200 °C | 311 - 392 °F | film blowing |
Premix Thermoplastics PRE-ELEC® CP 1319 PRE-ELEC CP 1319 is a conductive thermoplastic compound based on EVA. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC CP 1319 .. |
|||
Melt Temperature | 160 - 200 °C | 320 - 392 °F | |
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin
(discontinued **) LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Melt Temperature | 150 - 200 °C | 302 - 392 °F | Injection Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | Injection Molding |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Melt Temperature | 150 - 200 °C | 302 - 392 °F | Injection Molding |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 150 - 200 °C | 302 - 392 °F | Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 170 - 200 °C | 338 - 392 °F | |
Borealis FA3227 Low Density Polyethylene FA3227 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Heat and U/V stabilized. This grade is suitable for building construction film and meets the requirements for heat, al.. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
Eurostar Starflam MX05075 PP, Flame Retardant, Injection Molding Starflam MX05075 is an Unfilled Halogen Free Flame Retardant PP Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 190 - 200 °C | 374 - 392 °F | |
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene 70% Magnesium HydroxideFor extrusion of fire resistant aluminum composite panels.Information provided by PolyPlastic Group. |
|||
Melt Temperature | 140 - 200 °C | 284 - 392 °F | Average value: 173 °C Grade Count:22 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |