Polymer Property : Melt Temperature = 478 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA73MP is a lubricated and nucleated low viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 C..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA73ZP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA95MP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA95MP is a low viscosity nylon 6/6,6 copolymer extrusion grade. It conforms to Food and Drug Administration requirements of 21 CFR177.1500. Aegis HCA73ZP possesses the combinati..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA95QP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA95QP is a lubricated medium viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA95YP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA95YP is a lubricated medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA95ZP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA95ZP is a medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It p..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA115QP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500...
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA115ZP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA115ZP is a high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possess..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA155MP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA115MP is a lubricated and nucleated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21..
Melt Temperature 248 °C
478 °F
Cast Film
Honeywell Aegis™ HCA155QP Nylon 6/6,6 Extrusion Grade Copolymer  (discontinued **)
Description: Aegis HCA115QP is a lubricated high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500...
Melt Temperature 248 °C
478 °F
LCL-PR29
Intercontinental Polymers 132 PET Polymer Type - Semi-Dull, Flame Retardant, Polyester Pellets
Applications: Fire Retardant (U.S) Filament SpecialtiesInformation provided by Intercontinental Polymers.