Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 220 - 255 °C | 428 - 491 °F | Start Point: 230°C |
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation .. |
|||
Melt Temperature | 235 - 255 °C | 455 - 491 °F | Start Point: 250°C |
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2100 PBT+GF10% Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2200 PBT+GF20% Description: Injection Molding, PBT+GF20%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2152 PBT+GF15% Description: Injection Molding, PBT+GF15%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5102F PBT+PC+GF10% Description: Injection Molding, PBT+PC+GF10%, Low Warpage, Flame RetardantApplication: IT/OA, E&E (Switch)CAS No. 9003-01-04, 68928-70-1, 65997-17-3, 24968-12-5, 103598-77-2 and 1309-64-4Information.. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® LW5402A PBT+PC+GF40% Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® SG3180S PBT+PET+MF18% Description: Injection Molding, PBT+PET+MF18%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® GP2306FY PBT+GF30% Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided .. |
|||
Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
LG Chemical Lupox® HI2303 PBT+GF30% Description: Injection Molding, PBT+GF30%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |