Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 282 - 304 °C | 540 - 579 °F | |
PolyOne Stat-Tech™ PC-15CF/000 Black Polycarbonate (PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Melt Temperature | 282 - 321 °C | 540 - 610 °F | |
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy. Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural off-whit.. |
|||
Melt Temperature | 282 - 321 °C | 540 - 610 °F | |
Oxford Polymers PPS/66-505-40GF-BK PPS/PA66, 40% Glass Fiber Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy with Nylon 66 Processing and Delivery Form: Pellets and Injection MoldingAppearance: Bla.. |
|||
Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Melt Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
Polymer Resources PPX-GP2 Modified PPO, General Purpose with HDT of 250 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 282 - 310 °C | 540 - 590 °F | |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Melt Temperature | 282 - 299 °C | 540 - 570 °F | |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Melt Temperature | 282 - 343 °C | 540 - 650 °F | Average value: 315 °C Grade Count:32 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Melt Temperature | 282 - 304 °C | 540 - 580 °F | |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Melt Temperature | 282 °C | 540 °F | |
Chem Polymer Chemlon 125 G Nylon 66, 25% Glass Sphere Reinforced A 25% glass sphere reinforced nylon 66 offering a balance of rigidity, dimensional stability and surface appearance.Data provided by the manufacturer, Chem Polymer. |