Polymer Property : Melt Temperature = 559 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 271 - 293 °C
520 - 559 °F
PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 266 - 293 °C
511 - 559 °F
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 271 - 293 °C
520 - 559 °F
PolyOne Gravi-Tech™ GRV-NY-050-CU-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 271 - 293 °C
520 - 559 °F
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 271 - 293 °C
520 - 559 °F
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66)
Property data for molded test bars: Dry as MoldedInformation provided by PolyOne
Melt Temperature 260 - 293 °C
500 - 559 °F
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 271 - 293 °C
520 - 559 °F
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 271 - 293 °C
520 - 559 °F
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melt Temperature 277 - 293 °C
531 - 559 °F
Styron EMERGEâ„¢ 4510-15 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
Melt Temperature 277 - 293 °C
531 - 559 °F
Styron EMERGEâ„¢ 4530-15 Polycarbonate
EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
Melt Temperature 277 - 293 °C
531 - 559 °F
Eastman Eastar EN076 Copolyester
Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o..
Melt Temperature 277 - 293 °C
531 - 559 °F
Eastman Eastar MN058 Copolyester
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra..
Melt Temperature 277 - 293 °C
531 - 559 °F
Eastman Eastar MN059 Copolyester
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra..
Melt Temperature 277 - 293 °C
531 - 559 °F
Eastman Eastar EN059 Copolyester, Natural
Applications:Cosmetics/personal care packagingDeodorant PackagingFragrance packagingOral hygienePlastics for hygiene feminine productsToothbrushesToys/Sporting goodsWriting instrumentsProduct Descri..
Melt Temperature 271 - 293 °C
520 - 559 °F
Stock
PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber  (discontinued **)
Data provided by PolyOne.
Melt Temperature 271 - 293 °C
520 - 559 °F
Stock
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Melt Temperature 271 - 293 °C
520 - 559 °F
Stock
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Melt Temperature 271 - 293 °C
520 - 559 °F
Stock
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Melt Temperature 260 - 293 °C
500 - 559 °F
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued
12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..