Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | Injection |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | Injection |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH
(dis AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9530 PPS, 55% Mineral
(discontinued **) Good-flow Embedding Compound, Isotropic Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Embedding of Microchips and Electronic ComponentsProcessing: Inject.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9561 PPS, 60% Glass Fiber/Mineral
(discontinued **) High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral
(discontinued **) Mineral-filled Grade with Improved Impact Strength, Low Mold Temp. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Shaft Seals, FlangesProcessing: Injection Molding (M.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Melt Temperature | 321 - 335 °C | 610 - 635 °F | |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Melt Temperature | 321 - 338 °C | 610 - 640 °F | |
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Melt Temperature | 321 - 329 °C | 610 - 624 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Conditioned) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Melt Temperature | 321 - 345 °C | 610 - 653 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L 9560 PPS, 50% Mineral High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje.. |
|||
Melt Temperature | 321 - 335 °C | 610 - 635 °F | |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Melt Temperature | 321 - 360 °C | 610 - 680 °F | |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
Melt Temperature | 321 - 341 °C | 610 - 646 °F | Injection |
Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber
(discontinued **) High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fan Blades, Brake Sleeves, Model Constructi.. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of .. |
|||
Melt Temperature | 321 - 343 °C | 610 - 649 °F | |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |
|||
Melt Temperature | 321 - 338 °C | 610 - 640 °F | Injection |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded
  AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |
|||
Melt Temperature | 321 - 338 °C | 610 - 640 °F | Injection |
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, at 50% RH
(di AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela.. |
|||
Melt Temperature | 321 - 338 °C | 610 - 640 °F | Injection |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |