Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 371 - 399 °C | 700 - 750 °F | Molding |
PolyOne Edgetek® PK-1000 Polyetheretherketone (PEEK)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 332 - 399 °C | 630 - 750 °F | Average value: 371 °C Grade Count:3 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Melt Temperature | 20.0 - 399 °C | 68.0 - 750 °F | Average value: 276 °C Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Melt Temperature | 349 - 399 °C | 660 - 750 °F | |
Clariant Renol PEEKSP0002 Polyetheretherketone, 30% Glass Fiber Data provided by Clariant Masterbatches |
|||
Melt Temperature | 354 - 399 °C | 670 - 750 °F | Average value: 380 °C Grade Count:4 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Temperature | 343 - 399 °C | 649 - 750 °F | |
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |