Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000322 ohm-cm | 0.00000322 ohm-cm | (52% IACS) |
CMW® ELKONITE® 3042 Silver Tungsten Carbide contact material ASTM B663 For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |