Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Hogen Duralloy H10W 75 Tungsten/25 Copper PM Metal Composite RWMA Class 11.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a hard.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Hogen Duralloy H20W 78 Tungsten/22 Copper PM Metal Composite RWMA Class 11 and 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 mater.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection weld.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Mi-Tech Metals CW78 78 Tungsten/22 Copper PM Metal Composite RWMA Class 11 and 12.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is .. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Mi-Tech Metals TC50 50 Tungsten Carbide/50 Copper PM Metal Composite Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection welding die.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Mi-Tech Metals CW75 75 Tungsten/25 Copper PM Metal Composite RWMA Class 11.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a harder mate.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Alcoa UltrAlloy® 6020-T8 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | |
Alcoa UltrAlloy® 6020-T9 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | 47 % IACS |
CMW® ELKONITE 30SB tungsten, silver Information provided by CMW Inc. |
|||
Electrical Resistivity | 0.00000370 ohm-cm | 0.00000370 ohm-cm | (55% IACS) |
CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |