Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 424 Type III, I-F Enamel Enameling Carbon Steel I-F Enameling Steel is a vacuum degassed, titanium stabilized steel. I-F Enameling Steel can be used for ground coat and two coat-one fire porcelain enameling systems. It is not recommended for us.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 570, Grade 30 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 570, Grade 36 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 607 Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 607 Class 1 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 1 has limits placed on C, Mn, P and S with a 15 ksi difference between the minimum spec.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 607 Class 2 Formable, Grade 45K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA) ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. .. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 907, Grade 33 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel CL 1/ SAE J1392 045 XLK, Grade 45 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel Cold Rolled Carbon Steel, Dent Resistant (DR 180), SAE J2340 Type 180 A Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel Cold Rolled Carbon Steel, Dent Resistant (DR 210), SAE J2340 Type 210 A Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel Grade 30 Cold Rolled Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel Hot Rolled Carbon Steel, Drawing Steel with Boron (DS Type B), Standard Grade DS is made by adding aluminum and boron to the molten steel and may be used in severe drawing applications.Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel SAE J1392 040XLK or 040YLK, Grade 40 Cold Rolled Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® 255, Grade 37 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® 275, Grade 40 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® Class 2, Grade 50 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Commercial Steel (CS Type B), Standard Grade May be moderately formed. A specimen cut in any direction can be bent flat on itself without cracking.Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Steel, Bake Hardenable (BH 180) Brake Hardenable steels offer good formability and an increase in strength after paint bake.Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Deep Drawing Steel (DDS Type B), Standard Grade Made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 045XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, High Strength Low Alloy Steel (HSLA), 055XLK SAE Specified properties not covered by ASTMInformation provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ASTM A 570, Grade 50 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® 230, Grade 33 Hot Dip Galvanized Carbon Steel, Structural Steel (SS) Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium to the molten steel after degassing and offer excellent drawability.Information provided by AK Steel |
|||
Electrical Resistivity | 0.0000142 ohm-cm | 0.0000142 ohm-cm | |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Bake Hardenable (BH 250) Information provided by AK Steel |