Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Poco Graphite AXF-5Q10W Biomedical Grade Graphite POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Heraeus Cleviosâ„¢ P Jet 700 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet 700 is an antistatic material based on P.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-400 1K HTA-7W EP01 Continuous Filament Carbon Fiber Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 12K HTA-7C NS01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 3K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 3K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 3K HTA-7W EP01 Continuous Filament Carbon Fiber Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-700 12K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-700 12K HTA-7C F301 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-700 24K HTA-7D F402 Continuous Filament Carbon Fiber Standard Modulus; Wide Band; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carb.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® STS 24K HTA-7C F301 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Electrical Resistivity | 0.00150 ohm-cm | 0.00150 ohm-cm | |
Toho Tenax Besfight® G30-500 12K HTA-7S F202 Continuous Filament Carbon Fiber Standard Modulus; Soft Wide Band; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |