Electrical Properties Metric English Comments
Electrical Resistivity 0.800 ohm-cm
0.800 ohm-cm
particle size 40 um, pressure 2.5 t/cc
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 0.800 ohm-cm
0.800 ohm-cm
particle size 40 um, pressure 2.5 t/cc
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 0.800 ohm-cm
0.800 ohm-cm
particle size 40 um, pressure 2.5 t/cc
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 0.800 ohm-cm
0.800 ohm-cm
particle 40 um, pressure 2.5 t/cc
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 0.800 ohm-cm
0.800 ohm-cm
Particle size 40 um, pressure 2.5 t/cc
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..