Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | particle size 18 um, pressure 2.5 t/cc |
TIMCAL TIMREX® GB98/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | particle size 18 um, pressure 2.5 t/cc |
TIMCAL TIMREX® GB99/6 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | particle size 15 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | particle size 15 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | particle size 15 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | particle 15 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 1.45 ohm-cm | 1.45 ohm-cm | Particle size 15 um, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |