Electrical Properties Metric English Comments
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 142 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS5-44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS5-75TT Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Electrical Resistivity 1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
TIMCAL TIMREX® KS75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..