Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Average value: 500000 ohm-cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM D257
PolyOne Edgetek® AS-10CF/000 ABS - 10% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 100 - 1.00e+17 ohm-cm
100 - 1.00e+17 ohm-cm
Average value: 5.11e+15 ohm-cm Grade Count:37
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 1.42e+16 ohm-cm Grade Count:81
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Electrical Resistivity 100 - 1.30e+13 ohm-cm
100 - 1.30e+13 ohm-cm
Average value: 1.00e+12 ohm-cm Grade Count:5
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Electrical Resistivity 100 - 1.00e+17 ohm-cm
100 - 1.00e+17 ohm-cm
Average value: 5.00e+16 ohm-cm Grade Count:9
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Electrical Resistivity 100 - 5.00e+16 ohm-cm
100 - 5.00e+16 ohm-cm
Average value: 1.25e+15 ohm-cm Grade Count:86
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 7.19e+16 ohm-cm Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 4.11e+16 ohm-cm Grade Count:70
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone
Electrical Resistivity 100 ohm-cm - 1e+05
100 ohm-cm - 1e+05
ASTM C611
Techmer ES Electrafil® J-50/CF/20/TF/15 Polycarbonate, 20% Carbon Fiber Reinforced, 15% PTFE
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 9.90e+9 ohm-cm
100 - 9.90e+9 ohm-cm
Average value: 6.61e+8 ohm-cm Grade Count:19
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Electrical Resistivity 100 - 1.00e+16 ohm-cm
100 - 1.00e+16 ohm-cm
Average value: 5.17e+15 ohm-cm Grade Count:6
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..