Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 150 - 1.63e+16 ohm-cm | 150 - 1.63e+16 ohm-cm | Average value: 1.63e+15 ohm-cm Grade Count:102 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Electrical Resistivity | <= 150 ohm-cm | <= 150 ohm-cm | |
Unipetrol A High-Conductive Carbon Black Chezacarb Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not .. |
|||
Electrical Resistivity | 150 ohm-cm | 150 ohm-cm | 8% graphite |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | <= 150 ohm-cm | <= 150 ohm-cm | |
Unipetrol B High-Conductive Carbon Black Chezacarb Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not .. |