Polymer Property : Dielectric Breakdown = 7000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 7000 V

@Thickness 1.57 mm
7000 V

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S/S
Industrial Laminates/Norplex NP634 Laminate
Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and..
Dielectric Breakdown 7000 V

@Thickness 0.250 mm
7000 V

@Thickness 0.00984 in
CeramTec Rubalit® 708S Alumina, 96%
Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste..
Dielectric Breakdown 7000 V

@Thickness 0.250 mm
7000 V

@Thickness 0.00984 in
ASTM-D149
CeramTec CeramCool® Rubalit® 708 Alumina, 96%
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..