Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Murtfeldt Murinit® SP Polyphenylene Sulfide Thanks to the low fiber content and integrated solid lubricant, Murinit® SP offers an excellent combination of good slide and wear behavior, high strength, and dimensional stability – even at high.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 1000 PE-UHMW, Natural OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | |
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60094 |
Manifattura Cattaneo PVDF Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene Avantra® 585K is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical impact strength. Although Avantra® 585K can be processed by any method applicable.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax CCP PBT 1100-104S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Styrolution Luran® S KR 2859 ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Surface Resistance | >= 1.00e+13 ohm | >= 1.00e+13 ohm | IEC 60093 |
Styrolution PS 542N HIPS Styrolution PS 542N is an impact polystyrene with high heat resistance.Information provided by Styrolution |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Solvay TECHNYL® A 208F PA66, DRY Description: Unreinforced polyamide PA66, heat stabilized, high fluidity, fast cycling grade, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 208F offers three main advanta.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | DIN 53482 |
Polyram PlusTek PA303G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | |
Covestro Baydur® 110 FR Polyurethane Rigid microcellular RIM polyurethane material. Fast demold times; self releasing; long flow paths possible, therefore suitable for production of large moldings. Parts are injected through only one .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Barlog Plastics KEBATER BFA20 PBT, 20% glass fiber reinforced, flame retardant PBT-GF20 FRInformation provided by BARLOG plastics GmbH. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 93 |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
CENTROPLAST CENTROMID 6 GF 30 Polyamide 6 30% glass fiber The 30% glass fibre matrix adds very high strength and rigidity to this material. It has increased dimensional accuracy when hot. Can be used for rollers, belt pulleys and racks.Information provid.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Azoty Tarnow™ TARNOFORM 300 CI2 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 10% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Surface Resistance | 1.00e+13 - 1.00e+17 ohm | 1.00e+13 - 1.00e+17 ohm | Average value: 1.34e+16 ohm Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT005 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, High Flow and Lubri.. |