Electrical Properties Metric English Comments
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group RALUPOL® 4566 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Surface Resistance 50.0 - 1.00e+13 ohm
50.0 - 1.00e+13 ohm
Average value: 1.56e+11 ohm Grade Count:81
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Surface Resistance 48.0 - 1.00e+13 ohm
48.0 - 1.00e+13 ohm
Average value: 7.69e+11 ohm Grade Count:11
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
IEC 60093
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Surface Resistance 1.00e+9 - 1.00e+13 ohm
1.00e+9 - 1.00e+13 ohm
ASTM D257
PolyOne Edgetek® AS-1000 SD Unreinforced ABS - Antistatic Protection  (discontinued **)
Data provided by PolyOne.
Surface Resistance 1.00e+9 - 1.00e+13 ohm
1.00e+9 - 1.00e+13 ohm
ASTM D257
PolyOne Stat-Tech™ AS-15GF/000 SD ABS - 15% Glass Fiber Reinforced - Antistatic Protection  (discontinued **)&
Data provided by PolyOne.
Surface Resistance 1.00e+10 - 1.00e+13 ohm
1.00e+10 - 1.00e+13 ohm
Average value: 8.42e+12 ohm Grade Count:6
Overview of materials for Polyamide-Imide, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp..
Surface Resistance 1.00e+10 - 1.00e+13 ohm
1.00e+10 - 1.00e+13 ohm
Average value: 5.81e+12 ohm Grade Count:7
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
Average value: 7.00e+12 ohm Grade Count:3
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Surface Resistance 1.00 - 1.00e+13 ohm
1.00 - 1.00e+13 ohm
Average value: 2.00e+11 ohm Grade Count:40
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
Average value: 7.00e+12 ohm Grade Count:3
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
Average value: 5.50e+12 ohm Grade Count:4
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Surface Resistance 1.00e+11 - 1.00e+13 ohm
1.00e+11 - 1.00e+13 ohm
ASTM D257
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT
LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
ASTM D257
Supreme Petrochem SP 6411 1924 Light Stabilized Polystyrene
Characteristics Prevents dust patterns due to static charges High gloss Good flow Improved light fastness Processing Injection molding Extrusion Applications A/C and cooler grill Material Status..
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
ASTM D257
Supreme Petrochem SP 6425 9885 Abrasion Resistant Polystyrene
Characteristics Low friction, impact polystyrene to provide wear resistance and static charge dissipation Excellent gloss & molded appearance and weld line miscibility Easy flowing grade with good..
Surface Resistance 1.00e+10 - 1.00e+13 ohm
1.00e+10 - 1.00e+13 ohm
ASTM D257
Unitika UNILATE® 1 SC PET
Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot..
Surface Resistance 1.00e+9 - 1.00e+13 ohm
1.00e+9 - 1.00e+13 ohm
Average value: 1.54e+12 ohm Grade Count:13
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Surface Resistance 1.00e+10 - 1.00e+13 ohm
1.00e+10 - 1.00e+13 ohm
Average value: 4.31e+12 ohm Grade Count:35
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Surface Resistance 1.00e+10 - 1.00e+13 ohm
1.00e+10 - 1.00e+13 ohm
Average value: 3.58e+12 ohm Grade Count:14
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Surface Resistance 1.00e+12 - 1.00e+13 ohm

@Temperature 90.0 - 90.0 °C
1.00e+12 - 1.00e+13 ohm

@Temperature 194 - 194 °F
Average value: 5.50e+12 ohm Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..