Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.67e+13 ohm | 2.67e+13 ohm | |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |