Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.00e+14 ohm @Temperature 23.0 °C |
3.00e+14 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Surface Resistance | 3.00e+14 ohm @Temperature 23.0 °C |
3.00e+14 ohm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | |
Ineos ABS Lustran® PG 298 Key Features:UnfilledPlatableSuitable processing methods:Injection molding |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | |
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | ASTM D257 |
Styron EMERGEâ„¢ 8702 Polycarbonate EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Sorona® 3015GV BK001 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% based .. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good .. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based .. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE NC010 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | 50% RH, 500V; ASTM D257 |
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | 50% RH; 500V; ASTM D257 |
ALM PA 650 Nylon 12 SLS Prototyping Polymer Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines.. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | ASTM D257 |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | ASTM D257 |
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC
(discontinued **) QC-8704FR is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, an.. |
|||
Surface Resistance | 3.00e+14 ohm @Temperature 23.0 °C |
3.00e+14 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Surface Resistance | 3.00e+14 ohm @Temperature 23.0 °C |
3.00e+14 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Surface Resistance | 3.00e+14 ohm @Temperature 23.0 °C |
3.00e+14 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |