Electrical Properties Metric English Comments
Electrical Resistivity 0.000103 ohm-cm

@Temperature 21.0 °C
0.000103 ohm-cm

@Temperature 69.8 °F
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Electrical Resistivity 0.000103 ohm-cm

@Temperature 500 °C
0.000103 ohm-cm

@Temperature 932 °F
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..