Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 20.0 °C
0.000122 ohm-cm

@Temperature 68.0 °F
Haynes 617 Nickel Alloy Plate
Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed..
Electrical Resistivity 0.000122 ohm-cm

@Temperature 400 °C
0.000122 ohm-cm

@Temperature 752 °F
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)