Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Lexan® 2814R PC (Europe-Africa-Middle East) LEXAN 2814R is a high viscosity, 10% glass reinforced, flame retardant grade, especially developed to meet the CSTB M2 flammability rating. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC 4 |
PTS Tristar® PC-30GFR 30% Glass Reinforced Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Comparative Tracking Index | 100 - 175 V @Thickness 6.00 mm |
100 - 175 V @Thickness 0.236 in |
UL Rating PLC 4 (100-175 V) |
Covestro Makrolon® SF-800 Polycarbonate, Structural Foam
(discontinued **) Properties based on foam density of 0.90 g/cc.Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially.. |
|||
Comparative Tracking Index | 100 - 155 V | 100 - 155 V | Average value: 141 V Grade Count:5 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 1000V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in .. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2312 PEI 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2313 PEI 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region... |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Comparative Tracking Index | 100 V | 100 V | UL 746 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+PS LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 1212-2 6.4 |
Hippe EP CP 201 Cellulose Paper Reinforced Epoxy Resin - Sheet Used in electronic applications. Good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 1212-2 6.4 |
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe. |
|||
Comparative Tracking Index | 100 V | 100 V | CTI M; Solution B; IEC 60112 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Comparative Tracking Index | 100 V | 100 V | Test Liquid A; IEC 60112 |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |