Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 400 V | 400 V | |
Plastcom SLOVAMID 6 GF 25 FRG 5 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°.. |
|||
Comparative Tracking Index | 400 V | 400 V | |
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Comparative Tracking Index | 400 V | 400 V | |
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Comparative Tracking Index | 400 V | 400 V | Solution A; IEC 60112 |
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Comparative Tracking Index | 400 V | 400 V | |
Polimeri Europa EDISTIR N1461 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-03 High molecular weight general purpose polystyrene with good mechanical strength. Well suitable for injection mold.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | IEC 60112 |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
Sylvin Technologies 916V0 Black PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Comparative Tracking Index | 400 V | 400 V | Solution A; Ø 93x3mm; IEC 60112 |
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS) High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka.. |
|||
Comparative Tracking Index | 400 V | 400 V | IEC 60112 |
Styrolution Luran® 358 N SAN Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
DSM Akulon® K224-HG3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 400 V | 400 V | dry; IEC 60112 |
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15 15% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Comparative Tracking Index | 400 V | 400 V | IEC 60112 |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 400 V | 400 V | VDE 0303-P1, IEC 112 |
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass Characteristics: 30% glass fibre filled |
|||
Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | PLC 1 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® MO21 Polyester Film, 750 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Comparative Tracking Index | 400 - 499 V @Thickness 3.00 mm |
400 - 499 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Comparative Tracking Index | 400 - 599 V @Thickness 3.00 mm |
400 - 599 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | Average value: 546 V Grade Count:6 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Comparative Tracking Index | 400 V | 400 V | IEC 60112 |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
Comparative Tracking Index | 400 - 599 V @Thickness 3.00 mm |
400 - 599 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |