Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | PLC code 1; UL 746A |
SABIC Innovative Plastics Cycolac® MG37CR ABS High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | 400 V | 400 V | CTI 100; IEC 112 |
Nilit FRIANYL B63 HS-SG-GV2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Comparative Tracking Index | 400 V | 400 V | IEC 60112 |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Comparative Tracking Index | >= 400 V | >= 400 V | Solution A; IEC 60112 |
PolyOne Bergamid™ A70 G25 U-SO TM Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
Comparative Tracking Index | 400 V | 400 V | |
Polimeri Europa EDISTIR N1670 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,095-06 General purpose polystyrene with good flow and good heat resistance. Recommended for extrusion in blend with HIP.. |
|||
Comparative Tracking Index | 400 V | 400 V | |
Polimeri Europa EDISTIR N1671 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,095-06 General purpose polystyrene with good flow and good heat resistance for rapid set-up. To be used in injection mol.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | IEC 60112 |
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | Solution A; IEC 60112 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | Solution A; IEC 60112 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 V | 400 V | A solution |
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Comparative Tracking Index | 400 - 599 V | 400 - 599 V | PLC 1; UL 746A |
Mitsubishi Xantar® C CF 107 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Comparative Tracking Index | 400 V | 400 V | ASTM D257 |
Elastomer Engineering Elastamide 100 Elastomer Modified RIM Nylon 6 30% crystallinity. Information supplied by Elastomer Engineering. |
|||
Comparative Tracking Index | 400 V | 400 V | TS EN 60112 |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 400 V | 400 V | M; IEC 60112 |
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Comparative Tracking Index | 400 V | 400 V | |
Covestro Bayblend® KU 1-1446 Polycarbonate/ABS Blend Good cold impact strength and fuel resistance.Applications: Automotive industry (interior and body parts).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated fr.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Comparative Tracking Index | 400 V | 400 V | DIN IEC 112 / VDE 030 t1 |
Brueggemann Chemical Nyrim® 1000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Comparative Tracking Index | 400 - 599 V @Thickness 3.00 mm |
400 - 599 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Comparative Tracking Index | 400 - 599 V @Thickness 3.00 mm |
400 - 599 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |