Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PEI U1000 PEI, unfilled, extruded (ISO Data) Duratron U1000 PEI is an amber translucent (non-optical quality) amorphous thermoplastic material, offering high strength and heat resistance. It performs continuously to 170 °C, making it ideal fo.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data) FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® 703XL PA 6 + internal lubricant, cast (ISO Data) This high performance cast nylon 6 bearing grade provides an even better wear resistance than Nylatron NSM, combined with good pressure-velocity capabilities and a near zero level of “stick-slip”... |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | EOS/ESD S11.11 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data) This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Quadrant PC 1000 extruded (ISO Data) Quadrant Engineering Plastic Products is marketing non-UV-stabilized polycarbonate stock shapes under the trade name Quadrant PC 1000. It is a natural, “non-optical” industrial quality (clear, tra.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |
|||
Surface Resistivity per Square | >= 1.0e+13 ohm | >= 1.0e+13 ohm | IEC 60093 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |