Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 110 - 180 sec | 110 - 180 sec | Average value: 123 sec Grade Count:3 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Arc Resistance | 110 - 125 sec | 110 - 125 sec | Average value: 120 sec Grade Count:13 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, high flowApplications: A variety of cases and connectorsInformation provided by API-Kolon. Information provided by API-Kolon. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-20UV Polycarbonate, General Purpose, UV Stability Grade Features: UV Stability, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting Covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-30FRT12 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-30UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures/covers, Safety products, E & E parts, Household appl.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-40 Polycarbonate, General Purpose Features: Standard, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications, Le.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-50MRA Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-50UV Polycarbonate, General Purpose, UV Stability Grade Features: UV stability, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex K-75E Polycarbonate, Extrusion Grade Features: Extrusion, High viscosity, Natural transparentApplications: Sheets FilmsInformation provided by Kotec Corporation |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex KFR-30 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex KG-30F15 Polycarbonate, Wear Resistant, 30% Glass Fiber Reinforced Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex KGN-20MRA Polycarbonate, Flame Retardant, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex KGN-30MRA Polycarbonate, Flame Retardant, 30% Glass Fiber Reinforced Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Kotec Carbotex KV-30FD Polycarbonate, Food Grade Features: Food contact, Medium viscosity, Mold release, TransparentApplications: Household appliance, Kitchenware, Food packaging/containersInformation provided by Kotec Corporation |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Arc Resistance | 110 sec | 110 sec | Tungsten; ASTM D495 |
Samsung Cheil Industries Infino® SC-1220UR PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (.. |
|||
Arc Resistance | 110 sec | 110 sec | Practical Use (Water Absorption 2.4%); ASTM-D495 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 110 sec | 110 sec | Practical Use (Water Absorption 2.5%); ASTM-D495 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Toyobo T-400 Nylon, 15% Glass-Reinforced Key Feature: G.F. 15%Information provided by Toyobo Co., Ltd |
|||
Arc Resistance | 110 sec | 110 sec | Practical Use (Water Absorption 2.4%); ASTM-D495 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 110 sec @Frequency 1.00e+6 Hz |
110 sec @Frequency 1.00e+6 Hz |
ASTM D495 |
Chengdu Polyster KLX-G11 PC Film & Sheet PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant,.. |
|||
Arc Resistance | 110 sec | 110 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TA250G45 , 45% Glass Fiber Reinforced PA66, DAM 45% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | 110 sec | 110 sec | ASTM D495 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |