Polymer Property : Arc Resistance = 125 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 115 - 125 sec
115 - 125 sec
ASTM D495
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Arc Resistance 110 - 125 sec
110 - 125 sec
Average value: 120 sec Grade Count:13
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Arc Resistance 115 - 125 sec
115 - 125 sec
ASTM D495
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
Arc Resistance 75.0 - 125 sec
75.0 - 125 sec
Average value: 94.8 sec Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Arc Resistance 120 - 125 sec
120 - 125 sec
Average value: 124 sec Grade Count:5
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Arc Resistance 85.0 - 125 sec
85.0 - 125 sec
Average value: 109 sec Grade Count:8
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..