Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Cookson Group Plaskon® 440S Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Combines exceptional reliability with wide process latitude. This material is designed to encapsulate a wide range of semiconduc.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated .. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
IDI Composites 48-50 Thermoset Polyester, Molding Moderate strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Arc Resistance | 190 sec | 190 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Arc Resistance | 190 sec | 190 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TA210F Fast Crystallinity PA66, DAM Fast crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T14 General Purpose Molding Compound BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495-61 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Arc Resistance | 190 - 210 sec | 190 - 210 sec | ASTM D495-61 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC 5338 Mineral Filled, Glass Reinforced Polyester BMC 5338 molding compound is a mineral Filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, medi.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Resinoid 1320 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |