Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 100 dB | 100 dB | @ 10 GHz; Mil Std 285 |
Precision Polymer Engineering S70L Conductive Silicone Rubber Tan coloured, Silicone Rubber, 66-75 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber. Equivalent to Mil G 83528 Type D.Applications: Specially compounded to offer excellent .. |
|||
Shielding Effectiveness | 100 dB @Frequency 5.00e+8 Hz |
100 dB @Frequency 5.00e+8 Hz |
Mil std 285 procedure; Mil-G-83528 |
P & P Technology EC-Q(F) Fluorosilicone Elastomer P & P Technology material reference EC-Q(F) is a fluorosilicone elastomer with a Nickel/Graphite conductive filler. Per MIL-G-83528. It is dark green in color. The material is specially compounded t.. |
|||
Shielding Effectiveness | 100 dB @Frequency 2.00e+9 Hz |
100 dB @Frequency 2.00e+9 Hz |
Mil std 285 procedure; Mil-G-83528 |
P & P Technology EC-Q(F) Fluorosilicone Elastomer P & P Technology material reference EC-Q(F) is a fluorosilicone elastomer with a Nickel/Graphite conductive filler. Per MIL-G-83528. It is dark green in color. The material is specially compounded t.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+10 Hz |
100 dB @Frequency 1.00e+10 Hz |
Mil std 285 procedure; Mil-G-83528 |
P & P Technology EC-Q(F) Fluorosilicone Elastomer P & P Technology material reference EC-Q(F) is a fluorosilicone elastomer with a Nickel/Graphite conductive filler. Per MIL-G-83528. It is dark green in color. The material is specially compounded t.. |
|||
Shielding Effectiveness | 100 dB | 100 dB | |
Premix Thermoplastics PRESEAL 6070 Ag-Coated Glass Metal replacement is one of the fastest growing areas for conductive plastics. Plastics, with their lighter weight, good processability and optimal combination of mechanical properties have challeng.. |
|||
Shielding Effectiveness | 100 dB | 100 dB | |
Premix Thermoplastics PRESEAL 6070 Ag-Coated Glass Highly conductive PRESEAL® thermoplastic elastomer compounds are injection-mouldable and extrudable plastics for EMI-gasket and -housing applications, among other uses. The material is an ideal cho.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+7 Hz |
>= 100 dB @Frequency 1.00e+7 Hz |
E-Field |
P & P Technology KE Series Cored Shielding Mesh Gasket Strip Cover: Knitted Monel To BS 3075-NA 13 0.11mm Dia 2 Layers. Core Material: Neoprene closed cell sponge.Information provided by P & P Technology |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+7 Hz |
>= 100 dB @Frequency 1.00e+7 Hz |
E-Field |
P & P Technology KE Series Cored Shielding Mesh Gasket Strip Cover: Knitted Monel To BS 3075-NA 13 0.11mm Dia 2 Layers. Core Material: Neoprene closed cell sponge.Information provided by P & P Technology |
|||
Shielding Effectiveness | 100 dB | 100 dB | ASTM D790 |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Shielding Effectiveness | 100 dB | 100 dB | 20-700MHz; ARP1705 |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1291 Conductive Elastomer Commercial Grade Conductive Elastomer. This material is electronically conductive and specially formulated to provide shielding against electromagnetic interference. It is a high-performance Chomeri.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1291 Conductive Elastomer Commercial Grade Conductive Elastomer. This material is electronically conductive and specially formulated to provide shielding against electromagnetic interference. It is a high-performance Chomeri.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1291 Conductive Elastomer Commercial Grade Conductive Elastomer. This material is electronically conductive and specially formulated to provide shielding against electromagnetic interference. It is a high-performance Chomeri.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1291 Conductive Elastomer Commercial Grade Conductive Elastomer. This material is electronically conductive and specially formulated to provide shielding against electromagnetic interference. It is a high-performance Chomeri.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer Standard material for high volume injection and compression molding and small extrusions; high performance in non-corrosive environments; used in grounding applications with little or no vibration.R.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1356 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 10 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1356 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL E6434 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded onlyRoHS Compliant Information provided by C.. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 0.1 MHz - 10 GHz |
Parker Chomerics CHO-SHRINK® Heat Shrink EMI Shielding Conductive Heat Shrinking Shielding. CHO-SHRINK tubing is a heat shrinkable polyolefin tubing which provides effective EMI shielding for cables, connectors and cable/connector terminations. CHO-SHRI.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
>= 100 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
.25" x .375" Profiles; MIL-G-83528B |
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance .. |
|||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 500 MHz (E Field) - Base/Reinforced Material; MIL-G-83528 |
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |