Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 49 dB @Frequency 100000 Hz |
49 dB @Frequency 100000 Hz |
H-Field |
P & P Technology KE Series Cored Shielding Mesh Gasket Strip Cover: Knitted Monel To BS 3075-NA 13 0.11mm Dia 2 Layers. Core Material: Neoprene closed cell sponge.Information provided by P & P Technology |
|||
Shielding Effectiveness | 49 dB @Frequency 3.00e+7 - 1.00e+9 Hz |
49 dB @Frequency 3.00e+7 - 1.00e+9 Hz |
ASTM D149 |
Techmer ES Electrablend® ABS 03009 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Information provided.. |