Polymer Property : Dielectric Strength = 13.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 13.5 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
343 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
50%RH; Short Time; ASTM D149
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Dielectric Strength >= 13.5 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 342 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder
Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation ..