Polymer Property : Dielectric Strength = 25.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 25.3 kV/mm

@Thickness 1.60 mm
643 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East)
20% GF Super High Flow PBT