Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 559 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm,
Temperature 23.0 °C
559 kV/in

@Thickness 0.0630 in,
Temperature 73.4 °F
Short Time; ASTM D149
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Dielectric Strength 22.0 kV/mm

@Thickness 1.00 mm
559 kV/in

@Thickness 0.0394 in
Conditioned; IEC 60243-1
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers
PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 420SE0 PBT
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Valox® 701 PBT (Asia Pacific)
35% glass/mineral alloy, excellent electrical performance to dielectric breakdown. Developed for automotive distributor caps.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 815 PBT
15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East)
VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East)
VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009. 30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Dielectric Strength 22.0 kV/mm

@Thickness 1.60 mm
559 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E..
Dielectric Strength 22.0 kV/mm

@Thickness 0.800 mm
559 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific)
15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Dielectric Strength 22.0 kV/mm

@Thickness 2.00 mm
559 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.9%); ASTM-D149
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 22.0 kV/mm

@Temperature 23.0 °C
559 kV/in

@Temperature 73.4 °F
50%RH; IEC 60243-1
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66  (Unverified Data**)
Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information..
Dielectric Strength 22.0 kV/mm

@Temperature 100 °C
559 kV/in

@Temperature 212 °F
IEC 60243/1
BASF Ultramid® A3EG10 High Speed
Information provided by BASF
Dielectric Strength 22.0 kV/mm

@Thickness 2.00 mm,
Temperature 90.0 °C
559 kV/in

@Thickness 0.0787 in,
Temperature 194 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s..
Dielectric Strength 22.0 kV/mm

@Thickness 2.00 mm,
Temperature 90.0 °C
559 kV/in

@Thickness 0.0787 in,
Temperature 194 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..