Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 6.00e+15 ohm | 6.00e+15 ohm | Wet; after 16 hours at 130°C |
Malvern Minerals Diallylphthalate with Methallylate Silane Treated Novakup® 1250 Quartz Filler Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with 1.0% Z-6030 methallylate silane) filler. Separate entries demonstrate the effect of untreated NovaciteÂ.. |