Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C2951 PC+ABS (Asia Pacific) CYCOLOY C2951 is a flame retardant PC+ABS free from chlorinated or brominated flame retardant additives. High heat resistance is offered for demanding electrical applications, whilst maintaining exc.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL Rating PLC 0 (>120 arcs) |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
BK |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
High Amp Arc Ignition, HAI | 120 arcs | 120 arcs | Average value: 120 arcs Grade Count:3 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL Rating PLC 0 (>120 arcs) |
LG Chemical 81HF SAN Resin High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 4001 PEI PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 7500-105 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.05 mm |
>= 120 arcs @Thickness 0.120 in |
UL PLC 0 (120+ arcs) |
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific) VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific) GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | surface, PLC code 0; UL 746A |
SABIC Innovative Plastics Noryl PX1701 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL Rating PLC 0 (>120 arcs) |
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL Rating PLC 0 (>120 arcs) |
Covestro Makrolon® 2808 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |