Polymer Property : Dielectric Strength = 0.0787 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength <= 0.0787 kV/mm

@Thickness 1.59 mm
<= 2.00 kV/in

@Thickness 0.0625 in
Unconditioned; ASTM D149
Garlock 9850 Compressed Carbon Fiber Gasketing, Nitrile Binder
Carbon fibers with a nitrile binder.Carbon fiber gasketing excels in harshest conditions - intense heat, high pressure, saturated steam and hot oils.Laboratory-tested for fire safety.Long-lasting se..
Dielectric Strength <= 0.0787 kV/mm

@Thickness 1.59 mm
<= 2.00 kV/in

@Thickness 0.0625 in
Unconditioned; ASTM D149
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder
Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLo..
Dielectric Strength <= 0.0787 kV/mm

@Thickness 1.59 mm
<= 2.00 kV/in

@Thickness 0.0625 in
Unconditioned; ASTM D149
Garlock GYLON® 3530 PTFE Gasketing, Graphite Filler
PTFE with graphite fillerGraphite-filled PTFE offers extremely low void content for minimal emissionsBlack GYLON® delivers long service against volatile hazardous pollutants (VHAP and VOC)Withsta..