Polymer Property : Dielectric Strength = 10.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 10.3 kV/mm
262 kV/in
Short Term per ASTM D149.
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded  (discontinued **)
This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p..
Dielectric Strength 10.3 kV/mm
262 kV/in
Step by Step; ASTM D149
Plenco 1500 Polyester, Granular, Transfer Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..
Dielectric Strength 10.3 kV/mm
262 kV/in
Step by Step; ASTM D149
Plenco 1501 Polyester, Briquette, Compression Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Dielectric Strength 10.3 kV/mm
262 kV/in
Step by Step; ASTM D149
Plenco 3557 Phenolic, Granular, Compression Molded
PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r..
Dielectric Strength 10.3 kV/mm
262 kV/in
Short Time; ASTM D149
Plenco 3557 Phenolic, Granular, Transfer Molded
PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r..