Polymer Property : Dielectric Strength = 100 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 80.0 - 100 kV/mm
2030 - 2540 kV/in
ISO.243 DN.53481
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
Dielectric Strength 70.0 - 100 kV/mm
1780 - 2540 kV/in
ISO.243 DN.53481
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
Dielectric Strength 80.0 - 100 kV/mm
2030 - 2540 kV/in
ISO.243 DN.53481
Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high..
Dielectric Strength 18.5 - 100 kV/mm
470 - 2540 kV/in
Average value: 26.3 kV/mm Grade Count:49
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Dielectric Strength 16.0 - 100 kV/mm
406 - 2540 kV/in
Average value: 33.3 kV/mm Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Dielectric Strength 70.0 - 100 kV/mm
1780 - 2540 kV/in
ISO.243 DN.53481
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
Dielectric Strength 27.6 - 100 kV/mm
701 - 2540 kV/in
Average value: 54.8 kV/mm Grade Count:49
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Dielectric Strength 2.10 - 100 kV/mm
53.3 - 2540 kV/in
Average value: 34.5 kV/mm Grade Count:8
Overview of materials for Polytetrafluoroethylene (PTFE) Powder
This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Dielectric Strength 17.0 - 100 kV/mm
432 - 2540 kV/in
Average value: 33.0 kV/mm Grade Count:8
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Dielectric Strength 11.8 - 100 kV/mm
300 - 2540 kV/in
Average value: 29.3 kV/mm Grade Count:24
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Dielectric Strength 1.00 - 100 kV/mm
25.4 - 2540 kV/in
Average value: 33.0 kV/mm Grade Count:193
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Dielectric Strength 60.0 - 100 kV/mm
1520 - 2540 kV/in
DIN 53481
Isoflon TFM
Fluoropolymer material specifications.Information provided by Isoflon.
Dielectric Strength 12.0 - 100 kV/mm
305 - 2540 kV/in
Average value: 25.1 kV/mm Grade Count:53
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Dielectric Strength 13.0 - 100 kV/mm
330 - 2540 kV/in
Average value: 28.4 kV/mm Grade Count:20
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Dielectric Strength 14.0 - 100 kV/mm
356 - 2540 kV/in
Average value: 35.8 kV/mm Grade Count:10
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Dielectric Strength 17.0 - 100 kV/mm
432 - 2540 kV/in
Average value: 24.9 kV/mm Grade Count:28
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Dielectric Strength 11.8 - 100 kV/mm
300 - 2540 kV/in
Average value: 26.8 kV/mm Grade Count:105
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Dielectric Strength 15.0 - 100 kV/mm
381 - 2540 kV/in
Average value: 27.8 kV/mm Grade Count:48
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Dielectric Strength 19.7 - 100 kV/mm
500 - 2540 kV/in
Average value: 56.3 kV/mm Grade Count:5
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Dielectric Strength 15.0 - 100 kV/mm
381 - 2540 kV/in
Average value: 28.1 kV/mm Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved