Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | dry; IEC 60243-1 |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Dielectric Strength | 50.0 kV/mm @Thickness 0.533 mm, Temperature 23.0 °C |
1270 kV/in @Thickness 0.0210 in, Temperature 73.4 °F |
50% RH, ASTM D149-97a(04); ASTM D149 |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | ISO.243 DIN.53481 |
Omnia Plastica Arnite Omnialite POM c Acetal Copolymer Polyoxymethylene, commonly called Acetal, is a crystalline polymer obtained from the polymerisation of formaldehyde. Discovered fairly recently (1960), it has enjoyed rapid growth and large acceptan.. |
|||
Dielectric Strength | >= 50.0 kV/mm | >= 1270 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Dielectric Strength | >= 50.0 kV/mm | >= 1270 kV/in | ISO.243 DN.53481 |
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 500 PE 500: Polyethylenes with molecular weight higher than 500,000 gr/mol. POLIPOLEN® PE (POLYETHYLENE) is maintained from coke oven gas or from natural gas or from Ethene or Ethane which is produce.. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | DIN 53481 |
Isoflon FEP Fluorinated Ethylene Propylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | DIN 53481 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | at 100 Hz |
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |
|||
Dielectric Strength | 50.0 - 90.0 kV/mm | 1270 - 2290 kV/in | DIN 53481 |
Isoflon PEHD 300 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Dielectric Strength | >= 50.0 kV/mm | >= 1270 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 154 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | ASTM D877 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | ASTM D149 |
Westlake Plastics Norylux™ EN-265 Modified Polyphenylene Oxide Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1200 G at 50% RH Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LM-05 HX nat PA12 Product description: Grilamid LM-05 HX natural is a medium viscosity, heat-stabilized nanocomposite PA12 extrusion and injection molding grade. The special features of Grilamid LM-05 HX natural are:.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | ASTM D877 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Dielectric Strength | 50.0 - 80.0 kV/mm | 1270 - 2030 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Dielectric Strength | >= 50.0 kV/mm | >= 1270 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe POM Copolymer Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | |
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | |
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic.. |
|||
Dielectric Strength | 50.0 kV/mm | 1270 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® A.30 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner.. |
|||
Dielectric Strength | 50.0 - 70.0 kV/mm | 1270 - 1780 kV/in | DIN 53481 |
Isoflon PCTFE Polychlorotrifluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |