Polymer Property : Dielectric Strength = 1450 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 57.1 kV/mm
1450 kV/in
IPC TM-650 2.5.6.2
Arlon 85N Polyimide Laminate and Prepreg
85N is a polyimide and laminate prepreg system for PWBs requiring resistance to high temperature, both in process and in end-use application. Bromine-free chemistry provides thermal stability for a..