Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Short Term; ASTM D149 |
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet) |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.17 mm |
400 kV/in @Thickness 0.125 in |
|
Ineos Nova 5751 High Impact Polystyrene
(discontinued **) High flow, Good impact, USP Class VIApplications: Single service impact, Medical, Housewares, CompoundingProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwi.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Resin Technology Group TIGA 291-EX Grey Medium Viscosity Polyamide Epoxy Adhesive Mix ratio 1 to 1 by weight.Tiga 291 EX Grey is a medium viscosity polyamide/ epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance are desired. T.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | ASTM D149 |
Plenco 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 GF15 IM1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | 2.54 mm gap |
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GB36 IM1 BK 36% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 36% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF/M40 HS L 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedTPCI# 7395102Informat.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF25 L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Dielectric Strength | 15.7 kV/mm | 399 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in .. |
|||
Dielectric Strength | >= 15.7 kV/mm @Thickness 3.17 mm |
>= 400 kV/in @Thickness 0.125 in |
|
Master Bond EP37-3FLSP Optically Clear Epoxy Has Low Exotherm Description: Master Bond EP37-3FLSP is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. It fe.. |
|||
Dielectric Strength | 15.7 - 70.9 kV/mm | 400 - 1800 kV/in | ASTM D149 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
Tra-Con Tra-Bond F123 Color Keyed High Temperature Epoxy Adhesive TRA-BOND F123 is a fast cure, low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating sin.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
Tra-Con Tra-Bond FS443 Color Keyed Thixotropic Epoxy Adhesive TRA-BOND FS443 is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating s.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
Trelleborg Emerson & Cuming Stycast® 2072 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
Cytec (Conap) RN-1000 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 55580R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 56590R026 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data Represents typical values fo.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R31901R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 44572R010 0.010" (0.254 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberAppearance: Red silicone rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
Arlon 47571R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone Rubber Substrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on fibergl.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R31031R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1564 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for th.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R33099G028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R33979C028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Layer Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in p.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Short Term; ASTM D149 |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 44560R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Test run on 1/8" specimens. |
Loctite® Durabond® E-05CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |