Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
Quantum PVDF Information provided by Quantum Advanced Engineering Plastics |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | Short Term; 10 mil film; ASTM D149 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | 50 V/sec; ASTM D149 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | IPC TM-650 2.5.6.2 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
3M 7959MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
3M 9059MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Dielectric Strength | 63.0 kV/mm | 1600 kV/in | ASTM D149 |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |