Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East) GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 121 PC (Europe-Africa-Middle East) LEXAN 121 is a low viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® EXL6033 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with good processability.Very low temp. ductility, UV-Stabilized, UL94 V1 rated in white colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® HPS2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® ML104R PC (Europe-Africa-Middle East) LEXAN ML104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatibility inform.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® ML3400 PC (Europe-Africa-Middle East) LEXAN ML3400 is a medium viscosity, impact modified grade with improved chemical resistance. It passes the British Standard 2495 and 5361 solvent tests. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.00 mm |
432 kV/in @Thickness 0.118 in |
ASTM D149 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® FXD144R PC (Europe-Africa-Middle East) LEXAN FXD144R is a transparent/translucent medium viscosity grade for light diffusion effects. FDA compliant. Internal mold release. The color package may affect performance.This data was supplie.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or .. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | VDE 0303 |
GEHR Plastics PE-HD Polyethylene HDPE Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 1.91 mm |
432 kV/in @Thickness 0.0750 in |
|
Momentive Performance Materials RTV31 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
LG Chemical Lupoy 3010-30 Polycarbonate Resin Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | ASTM D149 |
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU) Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL PX1134 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1134 is an unfilled material with a Vicat B/120 of 120°C according ISO 306. NORYL PX1134 offers improved impact performance to meet the standard ECE dashboard impact tests in the automoti.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | IEC 60243-1 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | IEC 60243-1 |
Styron CALIBREâ„¢ 303-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 .. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Dielectric Strength | 17.0 kV/mm @Thickness 2.00 mm |
432 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Dielectric Strength | 17.0 kV/mm | 432 kV/in | IEC 243 |
Solvay Specialty Polymers Primef® 4002 40% GF PPS, High Fluidity Grade
(discontinued **) Used for injection molding of high performance parts. |